Contact us if document is not available
Sikagard®-62
2-PART EPOXY PROTECTIVE COATING
Sikagard®-62 is a two part, rigid, 100 % solids, coloured high build epoxy resin based protective coating. Suitable for hot and tropical climatic conditions.
- Total solid
- Good mechanical and chemical resistance
- High build
- Impervious to liquids
- Easy to mix and to apply
Contact us if document is not available
Usage
- Chemical resistant protective layer on concrete, structural cementitious mortars, epoxy cement, epoxy resin based products and steel
- Lining in storage tanks and silos
- Anti-corrosion coating on steel in food processing plants, sewage works, farms, agricultural enterprises, chemical and pharmaceutical facilities and beverage industry
Advantages
- Total solid
- Good mechanical and chemical resistance
- High build
- Impervious to liquids
- Easy to mix and to apply
Packaging
Part A | 3.75 kg drums |
Part B | 1.25 kg drums |
Colour
RAL 7032 (pebble grey), other on request
Product Details
SUSTAINABILITY
According USGBC LEED Rating Sikagard®-62 conforms to the requirements of LEED EQ Credit 4.2: Low – Emitting Materials: Paints & Coatings SCAQMD Method 304 - 91, VOC Content < 100 g/l
CERTIFICATES AND TEST REPORTS
Test report No. ALR-2402/9391, Suitability of non-metallic materials and products for use in contact with water intended for human consumption with regard to their effect on the quality of the water. The product was found to be non-toxic and comply with the BS 6920:2014 Specifications.
Composition
Epoxy resin
Shelf life
Part A: 18 months
Part B: 18 months
From date of production if stored properly.
Storage conditions
The packaging must be stored properly in original, unopened and undamaged sealed packaging, in dry conditions at temperatures between +5°C and +30°C. Protected from direct sunlight.
Density
Part A | ~1.45 kg/l |
Part B | ~1.02 kg/l |
Mixed resin ~1.37 kg/l
Density values determined at +23°C
Solid content by volume
~100 %
Shore D Hardness
~80 | (DIN 5305) |
Mechanical resistance
Taber Abraser | CS 10/1000/1000 | ~27 mg |
Taber Abraser | CS 17/1000/1000 | ~70 mg |
Tensile adhesion strength
> 1.5 N/mm2 to concrete | (ISO 4624) |
Temperature resistance
Exposure | Dry heat |
Permanent | +50°C |
Max. 7 d | +80°C |
Max. 12 h | +100°C |
Note: No simultaneous chemical and mechanical exposure.
Chemical resistance
Please contact Sika Technical Service for specific information.
Application
Mixing ratio
Part A : Part B = 3 : 1 (by weight)
Layer thickness
~0.2 mm per layer
Ambient air temperature
+8°C min. / +40°C max.
Relative air humidity
< 80 %
Substrate temperature
+8°C min. / +40°C max.
≥ 3°C above dew point, beware of condensation
Pot Life
Temperature | Time |
+10°C | ~30 min |
+20°C | ~20 min |
+30°C | ~10 min |
Waiting time to overcoating
Temperature | Min. | Max. | Full cure |
+10°C | ~30 h | ~3 d | ~14 d |
+20°C | ~10 h | ~2 d | ~10 d |
+30°C | ~6 h | ~1 d | ~5 d |
Consumption
~0.30 kg/m2 per layer
APPLICATION INSTRUCTIONS
SUBSTRATE PREPARATION
- The substrate must be sound and of sufficient compressive strength (minimum 25 N/mm2) with a minimum pull off strength of 1.5 N/mm2.
- The substrate must be clean, dry and free of all contaminants such as dirt, oil, grease, coatings and surface treatments, etc.
- Concrete substrates must be prepared mechanically using abrasive blast cleaning or scarifying equipment to remove cement laitance and achieve an open textured surface.
- Weak concrete must be removed and surface defects such as blow holes and voids must be fully exposed.
- Repairs to the substrate, filling of blowholes/voids and surface levelling must be carried out using appropriate products from the Sikafloor®, Sikadur® and Sikagard® range of materials.
- All dust, loose and friable material must be completely removed from all surfaces before application of the product, preferably by brush or vacuum.
MIXING
Prior to mixing stir part A mechanically. When all of part B has been added to part A mix continuously for 3 minutes until an uniform mixed has been achieved. Use a low speed electrical stirrer (300 - 400 rpm) to avoid air entrapment. To ensure thorough mixing, pour materials into a clean container and mix again for at least 1,0 minute to achieve a smooth consistent mix. Excessive mixing must be avoided to minimise
air entrainment. During the final mixing stage, scrape down the sides and bottom of the mixing container with a straight edge trowel or spatula at least once to ensure complete mixing. Mix full units only.
APPLICATION
Prior to application, confirm substrate moisture content, relative air humidity, dew point, substrate, air and product temperatures.
Apply Sikagard®-62 onto the prepared substrate evenly using a roller, brush or airless spray at the required consumption rate.
CLEANING OF EQUIPMENT
Clean all tools with Thinner C immediately after use. Hardened and/or cured material can only be removed mechanically.